05-11-2017, 03:42 AM
Has anyone been able to or know how to print lower then 100um ? I have adjusted settings in my nanodlp settings but the prints turn out stretched only in the z hight resolution.

bolsoncerrado
05-11-2017, 08:16 AM
Thats weird. I print FDM resin at 75micron with no issues :??

vrogy
05-11-2017, 11:30 PM
I believe the X & Y will be linked right up to the pixel dimension of the LCD screen are thus fairly immutable.

Z seems like it should be able to be changed through a combination of curing time and stepper movement - with micro stepping and a 10 TPI leadscrew you're already into the ten thousandths of an inch positioning range.

Brickmaker
05-14-2017, 06:36 AM
do you use nanodlp? if so can you send me your setting?

RussellAnderson
12-04-2020, 04:04 PM
good site, I like it.

otis
09-06-2022, 03:51 AM
i also have this problem does anyone have a solution not only me with .